Sign In | Join Free | My entremaqueros.com |
|
Brand Name : TISCO, BAOSTEEL
Certification : ISO, SGS, BV
Place of Origin : China
MOQ : 1 ton
Price : Negotiation
Payment Terms : L/C, T/T
Supply Ability : 5000 Ton/Month
Delivery Time : Within 7-15 workdays after receiving deposit or L/C
Packaging Details : Standard Packing, or Per customer requirements
Name : ASTM/ASME SA179 SA192 Cold Rolled GI Steel Pipe for Boiler
Model NO. : CSP-010
Ends : Plain Ends
Coating Color : Black/ Oil
Transport Package : Protect with Ends Cap
Thickness : 2.77mm
Standard : ANSI B36.10
Application : Tubular Heat Exchangers, Condensers, and Similar Heat Transfer Apparatus
ASTM/ASME SA179 SA192 Cold Rolled GI Steel Pipe for Boiler and Heat Exchanger
1. ASTM A179 cold drawn seamless pipe manufacturers with thick dense zinc layer covered in the cold drawn seamless tube surface, it can avoid cold drawn seamless tube matrix and any contact with the corrosion solution to protect the steel matrix from corrosion. In the general atmosphere, the surface of the zinc layer to form a layer of thin and dense zinc oxide surface, it is difficult to dissolve in water, so the steel matrix plays a protective role. If zinc oxide and other components of the atmosphere produce insoluble zinc salt, the anti-corrosion effect is more desirable.
2. With iron - zinc alloy layer, combined with dense, and with the unique anti-corrosion in the marine atmosphere and atmospheric atmosphere.
3. ASTM A179 cold drawn seamless pipe with a strong wear resistance due to the combination of solid, zinc - iron miscible.
4. Since zinc has good ductility, its alloy layer and steel base attached to a solid, so hot-rolled parts can be cold, rolling, drawing, bending and other molding without damage to the coating.
5. Hot-dip galvanized structural steel pipe, the equivalent of an annealing treatment, can effectively improve the mechanical properties of steel matrix to eliminate the steel forming welding stress, is conducive to the steel structure for turning.
6. The surface of cold drawn seamless pipe after hot galvanized is bright and beautiful.
7. Pure zinc layer is the most hot galvanized layer of galvanized layer, its nature is basically close to pure zinc, with ductility, so it is full of flexibility.
Chemistry Composition:
C, % | Mn, % | P, % | S, % |
0.06-0.18 | 0.27-0.63 | 0.035 max | 0.035 max |
Mechanical Properties:
Tensile Strength, MPa | Yield Strength, MPa | Elongation, % | Hardness, HRB |
325 min | 180 min | 35 min | 72 max |
Outside Diameter & Tolerance
Outside Diameter, mm | Tolerance, mm |
3.2≤OD<25.4 | ±0.10 |
25.4≤OD≤38.1 | ±0.15 |
38.1 | ±0.20 |
50.8≤OD<63.5 | ±0.25 |
63.5≤OD<76.2 | ±0.30 |
76.2 | ±0.38 |
![]() |
ASTM ASME SA179 SA192 Cold Rolled GI Steel Pipe For Boiler And Heat Exchanger Images |